LINCOLN ELECTRIC K4680 Metal-Cored Wire Steel Spool 0.045 Dia, 786WF4

backorder
item
33VRH0455
Mfr ED031583
Rp. 4,661,000.00
item
K4680 Metal-Cored Welding Wire Material Carbon Steel Wire Type Metal-Cored Process Metal-Cored Welding (MCAW) Wire Diameter 0.045 in Tensile Strength (As Welded) 75 to 85 ksi (75 Percent Argon/25 Percent Carbon Dioxide) 80 to 90 ksi (90 Percent Argon/10 Percent Carbon Dioxide) Yield Strength (Minimum Required) 58 ksi Yield Strength (As Welded) 65 to 75 ksi (75 Percent Argon/25 Percent Carbon Dioxide) 70 to 80 ksi (90 Percent Argon/10 Percent Carbon Dioxide) Spool Type Steel Spool
Mfr ED031583
More Information
Item Reference786WF4
BrandLINCOLN ELECTRIC
Weight (lb)33
Length (in)12.125
Width (in)11.75
Height (in)4.5
Harmonization Code8311200000
Country of OriginCanada
K4680 Metal-Cored Welding Wire Material Carbon Steel Wire Type Metal-Cored Process Metal-Cored Welding (MCAW) Wire Diameter 0.045 in Tensile Strength (As Welded) 75 to 85 ksi (75 Percent Argon/25 Percent Carbon Dioxide) 80 to 90 ksi (90 Percent Argon/10 Percent Carbon Dioxide) Yield Strength (Minimum Required) 58 ksi Yield Strength (As Welded) 65 to 75 ksi (75 Percent Argon/25 Percent Carbon Dioxide) 70 to 80 ksi (90 Percent Argon/10 Percent Carbon Dioxide) Spool Type Steel Spool